Fig. 1

Download original image
LaFeO3 thin films surfaces observed by SEM: with a x30k magnification (a) LaFeO3-750, (b) LaFeO3-850, (c) LaFeO3-1000; with a x50k magnification: (d) sharp termination grains in LaFeO3-750 (e.g. white arrow in image (a)), (e) flat region in LaFeO3-750 (e.g. black arrow in image (a)), (f) image of LaFeO3-750 showing a crack (pointed out with white arrows), (g) LaFeO3-1000. As an example, the arrow in the image (b) points out to a droplet, i.e. elaboration artifacts.