Tl-2212 thin films annealed in a Al2O3 crucible and a steel container*
1
Shandong Jiaotong University, Department of Physics, Jinan, Shandong Province 250023, China
2
National Laboratory of Superconductivity, Institute of Physics, Chinese Academy of Sciences, PO Box 603, Beijing 100080, China
3
Shangdong Normal University, College of Physics and Electronics, Jinan, Shandong Province 250014, China
Corresponding author: Yich@sdjtu.edu.cn
Received:
21
March
2006
Revised:
12
September
2006
Accepted:
13
October
2006
Published online:
13
December
2006
Tl2Ba2CaCu2Oy(Tl-2212) thin films were fabricated on (001) LaAlO3 substrates by a two-step technique in a semi-closed aluminate crucible and a sealed steel container, respectively. First, the amorphous precursor films were deposited by the pulsed laser deposition (PLD) method, and then they were thalliated in different containers. Almost pure phase Tl-2212 thin films can be prepared in both of the containers. However, the as-annealed films show obvious differences in superconducting properties and microstructure.
PACS: 74.72.Jt – Other cuprates, including Tl and Hg-based cuprates / 74.78.Bz – High-Tc films
© EDP Sciences, 2006
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.