Optical properties of amorphous ZnO thin film prepared from boiled Zn thin film in ultra high pure water
Nano-Optoelectronics Research Laboratory, School of Physics, Universiti Sains Malaysia, 11800 Penang, Malaysia
a e mail: subashanmugan@gmail.com
Received:
21
October
2011
Revised:
23
April
2012
Accepted:
14
May
2012
Published online:
6
June
2012
Amorphous zinc oxide (a-ZnO) thin films were synthesized from RF sputtered Zn thin films. The conversion was performed by processing Zn thin film in ultra high pure water at 95°C in various process times (120–180 min). X-ray spectra revealed the presence of amorphous ZnO in the processed films. The calculated band gap was laid in between 3.25 and 3.2 eV. Non-linear behavior in I-V characteristics was observed for all films. The structural defects of a-ZnO were confirmed with PL and Raman studies. The synthesized films at 180 min were more oxygen deficient.
© EDP Sciences, 2012
Current usage metrics show cumulative count of Article Views (full-text article views including HTML views, PDF and ePub downloads, according to the available data) and Abstracts Views on Vision4Press platform.
Data correspond to usage on the plateform after 2015. The current usage metrics is available 48-96 hours after online publication and is updated daily on week days.
Initial download of the metrics may take a while.